Back to Article
Early-age chemical and autogenous shrinkage of cement pastes containing palm oil fuel ash at different water-to-binder ratios
World Journal of Civil Engineering and Architecture
| Vol 4, Issue 1
Table 3. Mixture proportions per 100 g of binder.
| Mixture | w/b | POFA (%) | Cement (g) | POFA (g) | Water (g) |
| P0-0.3 | 0.3 | 0 | 100 | 0 | 30 |
| P10-0.3 | 0.3 | 10 | 90 | 10 | 30 |
| P20-0.3 | 0.3 | 20 | 80 | 20 | 30 |
| P30-0.3 | 0.3 | 30 | 70 | 30 | 30 |
| P0-0.4 | 0.4 | 0 | 100 | 0 | 40 |
| P10-0.4 | 0.4 | 10 | 90 | 10 | 40 |
| P20-0.4 | 0.4 | 20 | 80 | 20 | 40 |
| P30-0.4 | 0.4 | 30 | 70 | 30 | 40 |
| P0-0.5 | 0.5 | 0 | 100 | 0 | 50 |
| P10-0.5 | 0.5 | 10 | 90 | 10 | 50 |
| P20-0.5 | 0.5 | 20 | 80 | 20 | 50 |
| P30-0.5 | 0.5 | 30 | 70 | 30 | 50 |