Table 16. Average mechanical characteristics of DP-reinforced bio-mortars obtained inthe bending and compression test.
| results | Average value | STD | results | Average value | STD | |||||
| 0 | 0 | 0 | 0 | 0 | / | 5.39 | / | / | 31.1 | / |
| 1 | 1 | 5 | 1 | 1 | 5.32 | 4.67 | 1.17 | 17.9 | 19.51 | 2.11 |
| 3.91 | 18.7 | |||||||||
| 4.68 | 21.9 | |||||||||
| 2 | 1 | 10 | 2 | 4 | 3.39 | 3,57 | 7.06 | 11.32 | 11.50 | 3.49 |
| 3.62 | 11.98 | |||||||||
| 3.54 | 11.20 | |||||||||
| 3 | 1 | 20 | 5 | 8 | 5.39 | 4.90 | 3.64 | 18.8 | 18.23 | 0.56 |
| 4.76 | 17.7 | |||||||||
| 4.76 | 18.1 | |||||||||
| 4 | 2 | 5 | 2 | 8 | 3.25 | 3.80 | 6.28 | 16.6 | 15.60 | 1.86 |
| 4.50 | 16.6 | |||||||||
| 3.77 | 13.4 | |||||||||
| 5 | 2 | 10 | . 5 | 1 | 2.72 | 2.80 | 1.86 | 18.6 | 16.20 | 4.10 |
| 3.02 | 16.4 | |||||||||
| 2.68 | 14.5 | |||||||||
| 6 | 2 | 20 | 1 | 4 | 3.64 | 3.96 | 2.99 | 13.0 | 13.18 | 1.41 |
| 4.23 | 11.9 | |||||||||
| 4.02 | 14.7 | |||||||||
| 7 | 5 | 5 | 5 | 4 | 6.81 | 7.70 | 0.81 | 32.6 | 33.53 | 0.42 |
| 8.40 | 36.2 | |||||||||
| 7.90 | 31.8 | |||||||||
| 8 | 5 | 10 | 1 | 8 | 5.99 | 6.43 | 2.47 | 28.46 | 27.97 | 0.43 |
| 6.00 | 27.79 | |||||||||
| 7.31 | 27.67 | |||||||||
| 9 | 5 | 20 | 2 | 1 | 4.35 | 4.14 | 0.76 | 21.00 | 21.33 | 0.55 |
| 5.73 | 21.96 | |||||||||
| 3.22 | 21.03 |